- Applied
2 to 4 microns (80 to 160
millionths in.) thickness
|
- No
changes needed for component
dimensions
- Applies
to Steel, Stanless Steel,
Titanium, Aluminum and Other
non-porous metals
|
|
|
|
- Uniform
thickness over 3-dimensional
component
|
- Uniform
performance on all component
surfaces
- Maintain
surface geometry
|
|
|
|
- "Cool"
application approximatly
300° F
|
- No
changes to metallurgical properties
|
|
|
|
|
|
- No
post-coating finishing needed
- Maintain
finish on polished surfaces
|
|
|
|
|
|
- Withstand
high contact stress with no
delaminating
|
|
|
|
|
|
- Will
not flake off
- Wears
as microscopic carbon
|
|
|
|
|
|
- Withstand
high contact stress
- Increased
wear life
|
|
|
|
|
|
- Reduced
frictional losses
- reduce
power input
- Increased
component life
- Eliminate
galling of mating surface
|
|
|
|
|
|
- Conduct
heat away from surface, reduce
potential for overheating
and galling
|
|
|
|
|
|